Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Does anyone know of any studies that have been done on diffe... - Mar 18, 2005 by Sr. Tech
KIC Thermal Its on the web site (just root around) There... - Mar 18, 2005 by
I have done few thermocouples using high lead solder, silver... - Mar 21, 2005 by ams
two ways to attach a thermocouple first with hig temperatur... - Mar 21, 2005 by
Where are people getting their high temp solder? I've found... - Mar 21, 2005 by
Doesn't everyone get it from their regular paste supplier? ... - Mar 21, 2005 by Darby
Try Radio Shack We have no significant financial interest... - Mar 21, 2005 by davef
Let's examine some scenarios: What if... ...No solder sa... - Mar 21, 2005 by
Aluminium tape adheres quite well and is not intrusive. I be... - Mar 30, 2005 by
Someone sells the T-couples that are in a rigid tube and the... - Mar 30, 2005 by URL