Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Do you know why my solder paste sticks to the squeegee so mu...
- Jun 27, 2005
by
What size paste roll do you have on your stencil? It should...
- Jun 27, 2005
by
RDR
Humidity level can play into this as well. Good blades will ...
- Jun 27, 2005
by
SuMoTe
We've talked about this previously on SMTnet. Try searching...
- Jun 27, 2005
by
davef
Hi,
Check to make sure your paste is not dried up, and it...
- Jun 28, 2005
by
Grant
We also had issues with paste sticking on our Trans Automati...
- Jun 29, 2005
by
jdumont
geb