Does anyone come across the problem of pcb turns yellowish c...
- Aug 08, 2005
by
Jim
Could the temperature of your reflow recipe be exceeding the...
- Aug 08, 2005
by
davef
Hi Jim,
What type of your PCB finish?
...
- Aug 08, 2005
by
Ktron
Hi Ktron,
I'm still waiting for my supplier to get back t...
- Aug 08, 2005
by
Jim
Hi Davef,
I'm suspecting that too! The recipe we are usin...
- Aug 08, 2005
by
Jim
Jim
Can you be more specific? What's going "yellow / bei...
- Aug 08, 2005
by
davef
Hi Davef,
After reflow, the pcb board turns yellowish col...
- Aug 08, 2005
by
Jim
Jim
Can you be more specific? What's going "yellowish" on...
- Aug 08, 2005
by
davef
Hi Davef,
The whole laminate turns yellowish.
...
- Aug 08, 2005
by
Jim
Td or Decomposition Temperature (the temperature that the ep...
- Aug 09, 2005
by
davef
Hi Davef,
I've found it. Very useful info. Thanks a lot.
...
- Aug 09, 2005
by
Jim