What is the best/most economical way to check the thickness ...
- Oct 06, 2005
by
jdumont
measure the board thickness before coat by a screw gauge, an...
- Oct 06, 2005
by
Humiseal 1B73 Acrylic, thanks for the suggestion.
...
- Oct 06, 2005
by
jdumont
Put a known thickness gage next to your boards to be coated....
- Oct 06, 2005
by
A wet film gage works best.
...
- Oct 06, 2005
by
URL
URL: Who are some suppliers of "wet film gage"?
...
- Oct 06, 2005
by
davef
There's a ton of em'. We used the one from Paul N. Gardner ...
- Oct 07, 2005
by
URL