Views: 4959
We are running this reflow oven and are trying to get up to ...
- Nov 21, 2005
by
Try Manix inc. I know they Support this Reflow Oven Model.
...
- Nov 21, 2005
by
This oven was not designed to support lead free temps.
I am...
- Nov 21, 2005
by
Sr. Tech
According to the documentation that I have, the oven should ...
- Nov 21, 2005
by
Guenther
Here is Manix web site:
...
- Nov 21, 2005
by
Well, according to Manix, this oven can run lead free, I hav...
- Nov 23, 2005
by
Guenther
To state whether an oven can or cannot "do lead free" very m...
- Nov 25, 2005
by
PeteC
They may tell you it will solder lead free,(and it may) but ...
- Nov 27, 2005
by
Sr. Tech
Guenther