Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3161
Not all but some new boards we have had solder joint problem... - Dec 14, 2005 by snaggletooth
See "black pad" and determine if that's what you have. ... - Dec 14, 2005 by RDR
Heavens to Murgatroyd, we agree with Russ that "black pad" c... - Dec 14, 2005 by davef
SNAGGLETOOTH HOLDS HIS HANDS UP, HAVING JUST REACHED THE EDG... - Dec 15, 2005 by snaggletooth
Snaggie Oxidized nickel is very tough to solder. Using t... - Dec 15, 2005 by davef
i would assume when the PCB planner and customer would speci... - Dec 16, 2005 by snaggletooth
Try paste flux instead.... oh yeah.. clean it as soon as it ... - Dec 16, 2005 by JAX