Hi Guys
I am new to SMT Line
Currently having a lot of p...
- Dec 15, 2005
by
aswsteven
What u meant by change every 1.5 day ( Expose to enviroment ...
- Dec 15, 2005
by
Hi
I mean once I open the jar and load into the print mach...
- Dec 15, 2005
by
aswsteven
Welcome.
A day and a half seems like a very long time to ...
- Dec 15, 2005
by
davef
A day and half is a life time for our solder paste, Almit V1...
- Dec 16, 2005
by
snaggletooth
Try to get a sample of Indium and give it a try......i happe...
- Dec 16, 2005
by
How about keeping a fridge near the line and only putting on...
- Dec 16, 2005
by
Rob
Rob
The typical warming or stabilization time for solder ...
- Dec 16, 2005
by
davef
Hi Dave,
Sorry, blonde moment.
For our prototype line...
- Dec 16, 2005
by
Rob
Hi Guys
My is in line system, printer DEK 265 stencil 4 m...
- Dec 17, 2005
by
aswsteven