Hi. I am trying to understand Tg and how it relates to refl...
- Dec 16, 2005
by
mdemos1
Tg is just a way to say when the board goes limp... or a qui...
- Dec 19, 2005
by
JAX
We agree with Jax. Tg of resin does not necessarily mean bet...
- Dec 19, 2005
by
davef
from what i know, Tg is important from thermal stresses poin...
- Dec 19, 2005
by