Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 10470
Certain paste mfg specify 6 hours paste thawing time to norm... - Feb 13, 2006 by sumxp
Why not use microwave oven, it would be faster ? Be caref... - Feb 13, 2006 by
I'd be curious if a microwave would activate the flux. I'd ... - Feb 13, 2006 by RFredericks
Sure, if your solder joints are reliabale after reflow. TZ ... - Feb 13, 2006 by
You can put metal in a microwave (at least you can mine) as ... - Feb 13, 2006 by Steve Thomas
Good morning, Solder paste softeners are designed to allo... - Feb 14, 2006 by Hypnotia
Pardon me for being so bold, but I still cannot understand t... - Feb 14, 2006 by Sr. Tech
Well, you don't want your paste to spoil! It'll give it a b... - Feb 14, 2006 by
sumxp