Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3029
Hello,
I am automating a process on our floor from wir...
- Feb 13, 2006
by
RFredericks
Some low residue [no-clean] flux residues are cleanable, oth...
- Feb 13, 2006
by
davef
I'd check around for a wire solder that doesn't leave as muc...
- Feb 13, 2006
by
Here are some cleaning chemistry companies that have product...
- Feb 13, 2006
by
PeteC
Cleaning no-clean is the pitts. If cleaning required migrat...
- Feb 13, 2006
by
I have used Indium SMQ 92 H (not the newer J flux type) It...
- Feb 15, 2006
by