Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3542
We have just purchased a humidity logger and I need to know ...
- Feb 16, 2006
by
I depends on your components, your ESD program, and the max ...
- Feb 17, 2006
by
ANSI-J-STD-001 says words to the effect: 18-30*C, 30-70%RH
...
- Feb 17, 2006
by
davef
We shoot for 35, but will take 30.
...
- Feb 17, 2006
by
Hmm... how about the people inside this room; working in thi...
- Feb 17, 2006
by
Mika
Where in the world are you? Is it naturally that dry and you...
- Feb 19, 2006
by
Steve Thomas
Geo E