Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3737
I have been looking at wave pallets with titanium inserts. I... - Feb 22, 2006 by John S
Hello John, There are some coatings for aluminum to elimina... - Feb 22, 2006 by
We used durastone, with a profile routed out to expose certa... - Feb 23, 2006 by Rob
Hi John We manufacture titanium component parts for wave ... - Feb 23, 2006 by Teilo Engineering Ltd
Hi, Last time we bought it, it came from Roechling: ... - Feb 23, 2006 by Rob
Hi John, I have used some wave fixtures with titanium inser... - Feb 23, 2006 by
Hi, We also only use Pentagon EMS, and they are very good... - Feb 23, 2006 by Grant
Hello John, I have not received the data from you. Please ... - Feb 23, 2006 by
Do you want some coating for aluminum? If so here you go. ... - Feb 23, 2006 by
I thought durastone was not ESD safe? ... - Feb 23, 2006 by
Hi Ken, There may be different composites of Durastone, b... - Feb 24, 2006 by Rob