Please advice how can we reduce a delta T of 40 degres betwe... - Mar 09, 2006 by CGO
First make sure that ALL of your fans and heaters are workin... - Mar 09, 2006 by RDR
Fans and Heaters are checked last week all o.k.Next step wil... - Mar 09, 2006 by CGO
What type of profile are you using (soak or straight ramp)? ... - Mar 09, 2006 by jdengler
CGO Assuming your system is performing well here are a few ... - Mar 09, 2006 by Marc
Ramp or Soak give us same Deta T (from 35 to 40).All probes ... - Mar 09, 2006 by CGO
What make of oven? ... - Mar 09, 2006 by
OMNIFLOW 7. ... - Mar 09, 2006 by CGO
Is there a way that you could plot the data points of your p... - Mar 09, 2006 by RDR
Ah, I have 3 of these ovens. Not bad ovens at all. You men... - Mar 10, 2006 by
Increase Soak time & Slow down line did reduced Delta T by 1... - Mar 10, 2006 by CGO
I hate to ask an obvious question, but are you sure all of y... - Mar 10, 2006 by Bman
Yes, All six new (LF ready kit) thermocouples are tested goo... - Mar 13, 2006 by CGO
I would try swapping the hottest & coolest thermocouples whe... - Mar 13, 2006 by
Wow, MOLE now sells "lead free" probes? ... - Mar 13, 2006 by
Well Im more of a wave guy but we had an employee in the eng... - Mar 14, 2006 by
I can see why he left. Not knowing your board or paste, but... - Mar 15, 2006 by