Hi,
We are about to change our wave over to lead free sol...
- May 18, 2006
by
What is your bath made out of?
...
- May 18, 2006
by
Are you talking a tin purge here?
...
- May 18, 2006
by
RDR
Hi,
The bath is titanium coated, and the machine is only ...
- May 18, 2006
by
Grant
We did a tin bath on ours but it was provided for free by Ni...
- May 18, 2006
by
adlsmt
I don't have any experinence with this, but my concern is th...
- May 18, 2006
by
Bman
Hi,
The tin flush is a good idea, and better than the sup...
- May 18, 2006
by
Grant
Hi,
One other thing, and it's weird to be replying to mys...
- May 18, 2006
by
Grant
"Solder alloy compositions are numerous but the most importa...
- May 18, 2006
by
Grant