Hi, We ran some boards and the girl on the line put in so... - Jun 16, 2006 by Grant
Hi Grant, I can't speak for reliability, I don't know how y... - Jun 16, 2006 by jbrower
Hi Grant, just my opinion, I think the concern could be r... - Jun 16, 2006 by
Hi, Reliability was what I was worried about. We have ... - Jun 16, 2006 by Grant
Hi Grant, I understand your concerns about the reliability.... - Jun 16, 2006 by Mika
There are plenty of studies on this subject. If the BGA can... - Jun 19, 2006 by
Hi, In our setup what we usually avoid is to use RoHS BGA o... - Jun 19, 2006 by
whats an x-rated tool?? sounds like something you can buy i... - Jun 19, 2006 by Slaine
Loco, I will look for that Motorola study. Personally, we h... - Jun 19, 2006 by suboc
Again, the verdict is mixed here as well, but from the semin... - Jun 20, 2006 by Samir Nagheenanajar
Under fill them. ... - Jun 20, 2006 by
This has been debated several times on this forum, but I hav... - Jun 20, 2006 by muse
Hi, That's a really interesting article, however one thin... - Jun 20, 2006 by Grant
Hi, What are your thoughts about the article saying that ... - Jun 20, 2006 by Grant
We all know those academic 'reliability studies' are very fo... - Jun 20, 2006 by davef
Finally found a link to the NPL report, good reading. ... - Jun 21, 2006 by
Hi Muse, what do you mean by "with a SAC Ball and SnPb Past... - Jun 21, 2006 by Amol Kane
Burn from dave on again Chunks! I agree with dave - get... - Jun 21, 2006 by Dr Shocker
Hi, That was another very interesting article posted. ... - Jun 21, 2006 by Grant
That is about what I gathered as well grant, if the pb part ... - Jun 21, 2006 by RDR
I see what you're saying - I'm not a process guru by any mea... - Jun 21, 2006 by muse
Unless it was an x-rated tool built by a woman. ... - Jun 21, 2006 by
Grant, The best rule is- "If it works don't touch it". W... - Jun 22, 2006 by Evtimov
Ha ha, very funny. Not as funny as our burn on YOU! ... - Jun 22, 2006 by Dr Shocker
Yesa yes Samir - you are stupid to form any other opinion bu... - Jun 22, 2006 by Dr Shocker
Oh yeah, I forgot about the great big burn of 2006 you and d... - Jun 22, 2006 by
Hi, Yes, I agree, and it seems like these studies were de... - Jun 22, 2006 by Grant
"We certainly live in a better world now." Regarding lead... - Jun 22, 2006 by Paul M.