I'm looking to solder a individual wire to each of the leads...
- Jul 10, 2006
by
We'd:
* Clamp vice grips on the leads to keep movement of t...
- Jul 10, 2006
by
davef
1) Use insulated wire & only strip back as much as you need ...
- Jul 11, 2006
by
Rob
30 gage wire and lap solder, you will have no issues.
...
- Jul 11, 2006
by
RDR
Mike ,
Look at ...
- Jul 12, 2006
by
HEAT SHRINK TUBING?
...
- Jul 13, 2006
by
Mike