Hi Folk, what is the possible cause for the components (e... - Jul 21, 2006 by CKH
Thinner stencil Russ ... - Jul 21, 2006 by RDR
hot/cold slump, print misregistration ... - Jul 21, 2006 by RFredericks
Paste too thick. Paste not aligned on pad. Part not aligne... - Jul 21, 2006 by
- Dirty stencil transfering paste from the stencil bottom. ... - Jul 24, 2006 by nodlac
It could be an over-zealous operator moving the IC with twee... - Jul 24, 2006 by Samir Nagheenanajar
Set-down height to low, iow, parts getting squashed too deep... - Jul 24, 2006 by Steve Thomas