Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3116
All,
We have a conveyor that uses an o-ring belt , this b...
- Aug 21, 2006
by
You can try Larrying .... I mean BUTTing them together and u...
- Aug 21, 2006
by
....or a soldering iron
...
- Aug 21, 2006
by
Rob
Chunks,
I figured you would know about O rings. :/
Try ...
- Aug 23, 2006
by
Sr. Tech
I think cyanoacrylate is the glue of choice for buna-n, but ...
- Aug 23, 2006
by
Steve Thomas
At a previous job we had a kit to splice the belts. It was ...
- Aug 23, 2006
by
jdengler
Super glue too. It's not just for sniffing anymore...
Do...
- Aug 23, 2006
by
Hi Jerry-
The belt splice kit we used were made by Eagle Be...
- Aug 24, 2006
by
nodlac
Hi, this is not a solution for your o-ring "belt" problem bu...
- Aug 26, 2006
by
aj