Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3018
Using no-clean flux going thru wave when comes out there is ...
- Aug 22, 2006
by
Hi Steve,
What type of flux? How do you apply it? What ...
- Aug 22, 2006
by
Sounds like a rosin flux. Is it sticky as well?
Russ
...
- Aug 22, 2006
by
RDR
Using Interflux IF2005, Have electrovert as well as new Nova...
- Aug 22, 2006
by
okay so both the 2005 formulas from interflux are clear alch...
- Aug 22, 2006
by
RDR
We agree with Russ. Your topside should be 100 - 130*C. Yo...
- Aug 22, 2006
by
davef
Steve