Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2633
Hi all,
If a component is rated as Peak Temperature 225 D...
- Oct 18, 2006
by
I thought that it was a worse case scenario. This is when yo...
- Oct 18, 2006
by
Darby
It's the max you can put them through before you can expect ...
- Oct 19, 2006
by
Rob
Time is also a factor, usually.
IIRC almost everytime I"ve ...
- Oct 19, 2006
by
Stephen
thanks for replies guys.
I have a nearly Full RoHS Compli...
- Oct 19, 2006
by
If you're talking about practical application who knows? If ...
- Oct 19, 2006
by
Steve Thomas
Don't confuse ROHS compliant with "able to take higher temps...
- Oct 19, 2006
by
Stephen
I agree with Stephen there! Or maybe we just didn't care eno...
- Oct 19, 2006
by
Darby
df