We've just started running a lot of double sided assemblies....
- Oct 31, 2006
by
That depends, W/S or No-Clean, SnPb or Pb Free?
...
- Oct 31, 2006
by
A Very Frazzled Man
SnPb No-Clean.
We've done it on bare boards with alcohol ...
- Oct 31, 2006
by
In my other, better equipped life, we'd wipe them down manua...
- Oct 31, 2006
by
Steve Thomas
We never run raw solder paste through our board cleaner, bec...
- Oct 31, 2006
by
davef
John S.: IPA is dangerous choice. Look here: ...
- Oct 31, 2006
by
davef
Dave, your points certainly have merit and I wouldn't make a...
- Nov 01, 2006
by
Steve Thomas
John,
As Dave says, never clean raw paste. Let it sit for a...
- Nov 02, 2006
by
Darby
John S.