Hi all, Last week I have noticed, that solder changed col... - Jan 15, 2007 by Adam
Check the temp of your pot. It may be getting cooler if you... - Jan 15, 2007 by Real Chunks
are you using composite pallets in the wave or oil/wax aroun... - Jan 15, 2007 by
I have checked pot temperature in different parts of solder ... - Jan 16, 2007 by Adam
We are using composite pallets for our boards. Regards A... - Jan 16, 2007 by Adam
Try to process the composite pallet through the wave without... - Jan 16, 2007 by
Sorry that answer never really gave you the reason and ways ... - Jan 16, 2007 by
You guys are all joking right?! There aren't any contaminat... - Jan 19, 2007 by
I thought the same thing but he did mention density. I thre... - Jan 19, 2007 by Real Chunks
Even the level of solder in the pot can have effect on your ... - Jan 19, 2007 by RDR
Add solder. ... - Jan 19, 2007 by
Thx guys, I'll check everything you mentioned, including sol... - Jan 22, 2007 by Adam