Hi,
I am process engineer of SMT production.
We have some ...
- Jan 17, 2007
by
The most likely cause is moisture vapor outgassing violently...
- Jan 17, 2007
by
Maybe,
but distance between Tantalum capacitor and BGA is a...
- Jan 17, 2007
by
Vladimir
Vladimir,
Phil J is right. Tantalum�s moisture vapor outg...
- Jan 17, 2007
by
Hypnotia
Thanks - I will try ASAP.
...
- Jan 17, 2007
by
hai, in our smt process we are facing the following problem....
- Aug 12, 2008
by
ramesh.r
Vladimir