Anyone have experience wave soldering rigid flex assemblies?...
- Apr 04, 2007
by
robgd3
Maybe more baking time is needed.
Topside board temp too ...
- Apr 04, 2007
by
PeteC
Rob: How do you rework blow-holes and pin-holes?
PTH plat...
- Apr 04, 2007
by
davef
Pete,
Top-side temp might be an issue. What's the easies...
- Apr 04, 2007
by
robgd3
The easiest, long term cheapest, and most accurate way to ...
- Apr 04, 2007
by
davef
Dave,
We're reworking with flux and solder. We're observ...
- Apr 04, 2007
by
robgd3
On finding baking recipes in the fine SMTnet Archive, your p...
- Apr 05, 2007
by
davef
Dave,
I've seen some instances of solder as you mentioned...
- Apr 05, 2007
by
robgd3
Please note that pin holes and blow holes are not always def...
- Apr 05, 2007
by