I ran a prototype last week with one of the above mentioned connectors on board.
During Inspection post reflow we noticed a solder ball had formed at the top of each leg.
We used a 5thou stencil with 10% reduction on the width but it seems that we are applying too much paste ? anyone run with these components?
aj...