Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3556
I'm new to the website so if I don't sound like I know what ... - Jul 12, 2007 by ScottD
Hi Scott, Hard to tell what kind of problem you really ha... - Jul 12, 2007 by Real Chunks
Canyou see this contamination? Is it solder beads, flux or ... - Jul 12, 2007 by jmelson
Are you talking about problems with your product or your SMT... - Jul 12, 2007 by SWAG
Sorry I have just started working in this industry so I am n... - Jul 13, 2007 by ScottD
wow, never heard of such a thing! Are you sure it's allways... - Jul 13, 2007 by Loco
Just starting and already responsible for product quality an... - Jul 13, 2007 by Real Chunks
The Contamination has proven to be pretty random, lots of st... - Jul 13, 2007 by ScottD
Oh, sure, on fine-pitch parts you need a microscope or at le... - Jul 13, 2007 by jmelson
Hi Scott, Here is another thought. Check your wave solde... - Jul 16, 2007 by Real Chunks