I want to get a collective opinion from the forum... I was ...
- Aug 23, 2007
by
garyr
Water soluable fluxes are quite hydroscopic. If you keep RH...
- Aug 23, 2007
by
davef
Solder balls with wave soldering can have different causes. ...
- Aug 24, 2007
by
Joris Groot Koerkamp
I agree with Joris. But to add to his comment, the type of ...
- Aug 24, 2007
by
Hussman
What about when using noclean and alcohol based fluxes? Cou...
- Aug 24, 2007
by
garyr
I would say no, unless your machine is in extremeconditions....
- Aug 24, 2007
by
Hussman
This is what I was thinking, but I am being beat up pretty b...
- Aug 28, 2007
by
garyr