We are having problem to develop lead-free (SAC305) reflow p... - Sep 07, 2007 by Roy
Change to through hole or hand solder. we are in the same b... - Sep 07, 2007 by James
Good afternoon, What is the difference between your cap a... - Sep 10, 2007 by Hypnotia
About 25C difference between the cap joint and the small ICs... - Sep 10, 2007 by Roy
Can you implement a longer soak? how many feet of heat do y... - Sep 10, 2007 by RDR
How big is the cap ? We successfully reflow caps that measur... - Sep 10, 2007 by Sr. Tech
Good afternoon, Oops. Quite huge difference I must say. B... - Sep 11, 2007 by Hypnotia