Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7952
Is normal DI rinse cycle enough to wash away all residue aft...
- Jan 18, 2008
by
Arun
Just what is delaminationg during testing?
Water washing ...
- Jan 21, 2008
by
davef
We see delamination at Mold compound to substrate interface ...
- Jan 21, 2008
by
Arun
In your situation, the issue is the compatibility of your fl...
- Jan 21, 2008
by
davef
Dave F....BOGUS BOGUS BOGUS What compatability issue could ...
- Jan 29, 2008
by
Bruce Barton
Bruce Barton:
We're not intending to suggest that anyone ...
- Jan 29, 2008
by
davef
Won't argure with you Davef, but guys who suggest totally un...
- Feb 03, 2008
by
Bruce Barton
Bruce: We know Arun is not cleaning the board properly. Arun...
- Feb 04, 2008
by
davef