Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2349
Hi all, what sort of magnification is fair to use when ev... - Feb 04, 2008 by aj
I would use the IPC 610 Mag guidelines: >1.0mm (0.039") 1.7... - Feb 04, 2008 by James
I recommend checking the IPC Stencil and Misprinted Board Cl... - Feb 04, 2008 by KKleinsmith