Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7441
Hi All, One PCBA failed test after went through the Shock... - Mar 12, 2008 by Sean
Why would a board failure related problem be a process probl... - Mar 12, 2008 by Real Chunks
You can say: The pad was lifted after reflow and prior to th... - Mar 12, 2008 by davef
Thanks Real Chunks and Davef...Yours input is valuable to me... - Mar 13, 2008 by Sean
ol' hege has got to agree with Chunks and Dave. Seems every... - Mar 14, 2008 by Hegemon
All, What if BGA solder crack do exist after the shock te... - Mar 15, 2008 by Sean
Hi All, Besides the above question, I have another one as... - Mar 17, 2008 by Sean