Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 10728
I am using TopazX2, placing 0603 caps with #72 FNC nozzles. ... - Jun 16, 2008 by DucHoang
Could it be from a dirty stencil, rather than from the pick ... - Jun 17, 2008 by robgd3
You need to adjust the air kiss. The machine blows a slight ... - Jun 17, 2008 by dwelch123
"The machine blows a slight amount of air after placement an... - Jun 17, 2008 by DucHoang
vo^ cai' tab pick vacuum% set at 30 and tab mount vacuum % s... - Jun 18, 2008 by GEM
You're barking up the wrong tree. Solder "splashes" are gen... - Jun 18, 2008 by Real Chunks
service manual for topaz-xII chapter 15 set vacuum chapter... - Jun 18, 2008 by GEM
Hi Russ/Dave/Allen, Is the solder splash and solder ball ... - Jul 22, 2009 by Umar