Hello,
we are having issues with two assemblies where the M...
- Jun 26, 2008
by
Mark
Depends on a few variables. Could be the part, your profile...
- Jun 26, 2008
by
Real Chunks
Check your pad spacing on the board. Look at the IPC specs f...
- Jun 26, 2008
by
Sr. Tech
The pad size is okay. I have also requested the manufacturer...
- Jun 26, 2008
by
Mark
Yes, try slowing it down. It will indicate if your ramp up ...
- Jun 26, 2008
by
Real Chunks
Hello Mark,
I would recommend to look again on the pads. ...
- Jun 26, 2008
by
gabriella
Hi Mark,
Are these lead free parts on a leaded process? If ...
- Jun 26, 2008
by
kevin