Dear all,
As far as I know hot tear or shrink hole defect...
- Aug 05, 2008
by
Sean
Dear All,
In order to understand the issue, pls review th...
- Aug 05, 2008
by
Sean
We agree that the squigglie part of the section of the BGA b...
- Aug 06, 2008
by
davef
Thanks Davef....How is this defect look like when it appear ...
- Aug 08, 2008
by
Sean
Hot tear occurs at the surface of the solder connection. The...
- Aug 08, 2008
by
davef
Ok,,,noted..Thanks for help...Rgds Sean
...
- Aug 08, 2008