I would like to have the opinion about the reflow / solderin...
- Apr 05, 2001
by
jmlasserre
Per our staff here at ACI.........
Higher Temperatures mayb...
- Apr 05, 2001
by
CAL
I concur with your second approach. A profile needs to be t...
- Apr 05, 2001
by
davef
CAL's word of caution is right on. We tend to stay in the 2...
- Apr 09, 2001
by
Steve Thomas