Views: 8362
Has anybody ever use this method to reclaim the solder from ...
- Oct 10, 2008
by
Pratyeka
Where did you get the gadget? at JC penney?...seriuosly, wit...
- Oct 13, 2008
by
George
For 15 years I have used a similar method, only I used two b...
- Oct 13, 2008
by
dwelch123
I got this thing at a major grocery store called Loblaws.
S...
- Oct 14, 2008
by
Pratyeka
I use this directly in the solder pot inside the wave machin...
- Oct 14, 2008
by
Pratyeka
The bread pans are stackable, same size at top but smaller a...
- Oct 14, 2008
by
dwelch123
Could you elaborate a bit? What is tin phos additive?
...
- Oct 21, 2008
by
Pratyeka
We're not sure the specifics that BLT Circuit Services Ltd r...
- Oct 23, 2008
by
davef
Thank you Dave and BLT, very informative replies.
...
- Oct 30, 2008
by
Pratyeka