Hi all, Looking for a solder preform supplier. Looking t... - Oct 14, 2008 by g cronin
Aim solder out of Rhode Island, contact your local Aim Distr... - Oct 14, 2008 by Steve
Indium makes them too. ... - Oct 16, 2008 by floydf
Kester makes them as well ... - Oct 16, 2008 by blnorman
I first heard of them from Alpha Metals. ... - Oct 16, 2008 by Stephen
I could never get them to work. ... - Oct 18, 2008 by Hussman