Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5399
We changed paste manufacturers rather recently and are now s...
- Dec 22, 2008
by
mfcat
Hi,
it seems like a glue problem to me. If you don't have...
- Dec 22, 2008
by
emil
As Emil says, it's 100% the glue! Your paste is not designe...
- Dec 22, 2008
by
Dirk Nuendyke
We run our process like that all the time paste then glue
w...
- Dec 22, 2008
by
WRONGWAY
The first question in solving the "ol' SMT component loss af...
- Dec 22, 2008
by
davef
Oh,I consider the process is wrong,it is stencil print paste...
- Dec 24, 2008
by
tang