Hi, I am trying to reduce some 0402 cap tombstones. Th... - Apr 15, 2009 by rtmitchell
I've had some luck with longer soak. Of course that was on a... - Apr 16, 2009 by kpm
We know virtually nothing about your process, but here's som... - Apr 16, 2009 by davef
have you try to change the stencil apertures to another figu... - Apr 17, 2009 by Armando_Gomez
Hi, follow up, Thanks to everyone that responded. We f... - Apr 17, 2009 by rtmitchell
I have a solution.... contact me by mail Vapor phase gives ... - Apr 18, 2009 by Alfred Moran
Low tombstone pastes have been around for 8-10 years. Talk t... - Apr 18, 2009 by davef
I like this suggestion the best as a "band aid", check out s... - Apr 18, 2009 by Bill West
Home plate design is great for avoiding beads and tombstonin... - Apr 21, 2009 by Viking
TOMBSTONING OF 0402 AND 0201 COMPONENTS: "A STUDY EXAMINING ... - Apr 24, 2009 by davef