Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5023
Hello,
since some days we are facing strange problem with S...
- Aug 31, 2009
by
d0min0
How do you go about and what happens when you rework the poo...
- Aug 31, 2009
by
davef
Have you profiled at the problem side of the part?
...
- Sep 01, 2009
by
isd.jww
davef
As for the repair :
- with hot air blower it is no...
- Sep 01, 2009
by
d0min0
Is the solder wetting to the pad, and not to the part? If s...
- Sep 01, 2009
by
robgd3
Because it's always the same terminal of the same part that ...
- Sep 03, 2009
by
isd.jww
Does the established joint still exist if once again re-touc...
- Sep 03, 2009
by
sachu_70
to summarize
- 3 components are placed on a single module ...
- Sep 03, 2009
by
d0min0
Before you rule out the profile, did you run an actual profi...
- Sep 19, 2009
by
profilingguru
Did you try pre-tinning your board on this suspect pad/s to ...
- Sep 22, 2009
by
cman
hello,
we are profiling with the pcb each day - results a...
- Sep 23, 2009
by
d0min0
Is it possible you are putting boards in the oven with littl...
- Sep 23, 2009
by
jdengler
that crossed our minds - overloading of the oven
but in re...
- Sep 24, 2009
by
d0min0
I had this issue a few years ago with Kingbright LED's. The ...
- Sep 24, 2009
by
Mark