Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6476
We are using LOCTITE 3606 HAVING torque 70 kgf.cm , but the ...
- Nov 22, 2009
by
SMT Process Engineer
We're not familiar with Loctite 3606.
Adhesive bond stren...
- Nov 23, 2009
by
davef
Solder paste & reflow the Bottom side.Use wave solder pallet...
- Dec 05, 2009
by
Nagesh
have you checked solder resist cure as this will cause the g...
- Dec 10, 2009
by
BLT Circuit Services Ltd
Inspect your dispensed or printed adhesive deposits 100%, ma...
- Dec 17, 2009
by
ToddF
We used Loctite 3609 and never had problems. If memory serv...
- Dec 21, 2009
by
Lynn Norman
Make sure you(not someone simply telling you) check that the...
- Dec 23, 2009
by
Stephen