Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 10579
I am concerned about a 'tarnishing' effect after moisture ba... - Apr 23, 2010 by Hegemon
Hegeman: So you receive these boards in seal moisture barrie... - Apr 23, 2010 by davef
Therein lies the issue. Unknown storage conditions before w... - Apr 23, 2010 by Hegemon
Hege: Sounds like this customer is a putz. Ask the putz to ... - Apr 24, 2010 by davef
We had one product that used immersion silver plating. Ther... - Apr 26, 2010 by blnorman
Obviously knowledge in this area is still in a bit of a 'flu... - Apr 26, 2010 by Hegemon