Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4678
who's achieved in soldering to IC sockets with such machines... - May 03, 2010 by Jacki
What is the issue that you have when soldering IC sockets wi... - May 03, 2010 by davef
We solder SMD sockets all the time with reflow. What are you... - May 11, 2010 by Shawn Vike
Hi Dave the issue is the sockets were deformed after solder... - May 13, 2010 by Jacki
Jacki: That's exactly what we need to know, so that we can ... - May 13, 2010 by davef
Thanks Dave I tried various sockts but all were failed.At S... - May 16, 2010 by Jacki
Why doesn't your leaded paste melt until you get it to 250*C... - May 17, 2010 by davef
Hi Dave at 250'C, the leaded solder was melted.As evaluatio... - May 18, 2010 by Jacki
OK. So, why do you have to heat it to 250*C to get it melt?... - May 18, 2010 by davef