Recently we have been placing and reworking quite a few Linear LGA DC converter modules. These are LGA packages with integrated passive components which become easily disturbed in reflow. Even with perfect bumping techniques on the LGA using the polyimde stencils unless the reflow profile is perfect the yields are much below normal.
Anyone share other ideas that have been tried?