lead frame with high temp tape OK to flux clean??| 27 July, 2010
Hi expert, we have one lead frame product proposed to send to flux clean recently. The problem here is the frame is attached with high temp tape. After flux cleaning the frame, the tape turns out deformed in which we think it was due to chemical reaction. Anyone mind to share how to overcome the problem?? since flux clean is unavoidable here. thx.