Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 21343
We having issues installing the Linear Tech LTM8023. We have... - Aug 30, 2010 by SMT-manufacturer
We currently use this devise in one of our designs with no i... - Aug 30, 2010 by Mark
Hi Mark, Thanks for your responce! The stencil thickness... - Aug 31, 2010 by SMT-manufacturer
Dear SMT Manufacturer, I am wondering if the device could h... - Sep 01, 2010 by Graham
Dear Graham, Moisture isn't the issue because we have don... - Sep 01, 2010 by SMT-manufacturer
Dear SMT Manufacturer, As moisture is eliminated as the cau... - Sep 01, 2010 by Graham
Dear SMT-manufacturer, I would recommend to also have other... - Sep 01, 2010 by sachu_70
Dear Sachu_70, During the tests we also checkt other devi... - Sep 01, 2010 by SMT-manufacturer
Seems interesting ... I am certain this could be resolved. B... - Sep 02, 2010 by sachu_70
Good. This is the right way to profile. Let me ask you, have... - Sep 02, 2010 by sachu_70
Just to add to my comments,solder joint voids do occur in LG... - Sep 02, 2010 by sachu_70
Voiding is tricky, but some pastes have flux residue that ca... - Sep 02, 2010 by f.murch@sbcglobal.net
I ment LF318. We have a power supply board that has 3 differ... - Sep 02, 2010 by Mark
Mark, Can you send some X-ray foto's of your LGA solderjo... - Sep 03, 2010 by SMT-manufacturer
You can reduce and almost eliminate voids and other paste re... - Sep 09, 2010 by Matt Kehoe