Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I am looking for a conformal coating to protect a PWB that w...
- May 16, 2001
by
Diane
Urethane and parylene have the best long term humidity resis...
- May 16, 2001
by
davef
Parylene is arguable the best conformal coating there is, un...
- May 17, 2001
by
blnorman
Diane