we encounter bubbles on silicone coating after oven curing.w... - Jul 04, 2011 by ricky
The three primary causes for bubble generation in solvent-ba... - Jul 04, 2011 by davef
1.The bubbles appear only after the oven curing.before curin... - Jul 04, 2011 by ricky
Is this an addition-cure silicone? We once had coating bubb... - Jul 05, 2011 by blnorman
We agree. As Bill says, given that you seem to have bubb... - Jul 05, 2011 by davef
Ricky What silicone coating are you using? Are you usi... - Jul 06, 2011 by Lou
we are using the silicone Dow Corning JCR6101UP. we use it ... - Jul 06, 2011 by ricky
Interesting stuff. I must admit that I am unfamiliar with th... - Jul 07, 2011 by Lou
According to the datasheet, this is a LED encapsulant, is th... - Jul 11, 2011 by blnorman