I had send my coating board to the test lab for adhesion coa... - May 09, 2012 by Umar
It's good that you're consistent. Troubleshooting an inconsi... - May 10, 2012 by davef
Hi Dave, Thanks on yoru prompt reply, Can help to shar... - May 17, 2012 by Umar
We us a lot of 1B31 it could be one of the most common coati... - May 18, 2012 by KaHrpr
Umar Chapter 7 of IPC-HDBK-830, Guidelines for Design, Se... - May 18, 2012 by davef
I'll chime in here as well. If you have adhesion problems, ... - May 18, 2012 by blnorman
I use Trace and certainly recommend them. I actually just ha... - May 31, 2012 by jdumont
I use Trace Labs and certainly recommend them. I actuall... - May 31, 2012 by jdumont
Hi Norman... Thansk on yoru input, actually my adhesion ... - Jun 01, 2012 by Umar
Neither the Omega meter nor the IC are officially "destructi... - Jun 01, 2012 by blnorman
Umar, it may never be solved. Some coatings just do not stic... - Jun 08, 2012 by Lou