I'm having an issue with a particular board we run in our wa... - May 21, 2012 by Chris
What is the lead protrusion? ... - May 21, 2012 by Carlos
Does the part seem to flow properly? Are your land patterns... - May 22, 2012 by Reese
Bridging Causes: Insufficient flux, excessive pre-heat, high... - May 22, 2012 by davef
Protrusion is 1 mm. ... - May 22, 2012 by Chris
What is the configuration of these 4 pins? Square or inlin... - May 22, 2012 by Patrick Bruneel
Square ... - May 22, 2012 by Chris
Forgot something how is the top fill on the connector? ... - May 22, 2012 by Patrick Bruneel
I can't see the fill as they are underneath the connector. ... - May 22, 2012 by Chris
Here is a picture. ... - May 22, 2012 by Chris
Sizzling would be hard to hear our machine has forced air pr... - May 22, 2012 by Chris
These are the hold down clips for the connector. I'll post ... - May 22, 2012 by Chris
Lead spacing is probably an issue here. It would be better ... - May 22, 2012 by Reese
The spacing, and the length as everything else on this board... - May 22, 2012 by Chris
Chris, If the short in the picture is parallel to the wav... - May 22, 2012 by Patrick Bruneel
Do you have anything else on this board with a similar land ... - May 22, 2012 by Reese
> Chris, > > If the short in the picture is para... - May 22, 2012 by Reese
I will give 90 deg turn a try, I want to say we've tried thi... - May 22, 2012 by Chris
Well no luck on the rotation, tried all directions to no ava... - May 22, 2012 by Chris
So it went from parallel to perpendicular with regards to th... - May 22, 2012 by Reese
Reese, no stayed perpendicular in regards to the wave, howev... - May 22, 2012 by Chris
Patrick, correct, no clean alcohol based. Machine is a Vito... - May 22, 2012 by Chris
Try trimming the leads to no more than 0.020" instead of 0.0... - May 23, 2012 by DeanM
Patrick and Dean, I'll try both suggestions in the next day ... - May 23, 2012 by Chris
I would suggest that the pad size vs lead length vs lead pit... - May 27, 2012 by josh
spacing is very tight but you should be able to get it right... - May 29, 2012 by aj
Yes, 45 degree will kill the shadowing effect. YOu can also... - May 31, 2012 by edmaya33
Try a simple solder mask. I use Chemtronics. A bottle is onl... - Jun 01, 2012 by W Medley
Tried fluxing, then letting it sit for an hour and then runn... - Jun 01, 2012 by Chris
Perhaps apply the through hole part, solder mask only one ba... - Jun 01, 2012 by W Medley